An FCC iron-carbon alloy initially containing 0.20 wt% C is

An FCC iron-carbon alloy initially containing 0.20 wt% C is

An FCC iron-carbon alloy initially containing 0.20 wt% C is carburized at an elevated temperature and in an atmosphere wherein the surface carbon concentration is maintained at 1.0 wt%. If after 49.5 h the concentration of carbon is 0.35 wt% at a position 4.0 mm below the surface, determine the temperature at which the treatment was carried out.